ASTM-D7786 Standard Test Method for Determining Enamel Holdout

ASTM-D7786 - 2013 R19 EDITION - CURRENT
Show Complete Document History

Document Center Inc. is an authorized dealer of ASTM standards.
The following bibliographic material is provided to assist you with your purchasing decision:

Standard Test Method for Determining Enamel Holdout
ORDER

Price:

$61.00        


Want this as a site license?

Scope

1.1 This standard provides a method for determining the holdout characteristics of a primer and topcoat coating application. A standard topcoat is used to determine the absorption characteristics of a primer. Enamel holdout can be measured as a difference in observed gloss of the topcoat over a primer, relative to the gloss of the same topcoat over a non-porous, smooth surface.

1.2 The standard is written in the context that the user will be evaluating the enamel holdout characteristics of a primer. Alternatively, the standard may be used as a method to evaluate the enamel holdout characteristics of primer/topcoat system where the primer is constant and different topcoats are used as test paints.

1.3 This standard may also be used for evaluation of paints other than primers as the first coat. In this alteration the user can test the enamel holdout characteristics of a self-primed topcoat, or use of any other type of paint as the primer followed by the use of a standard topcoat.

1.4 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.6 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

Significance and Use

5.1 This standard may be used by paint companies and raw material suppliers to assess the interactions of primers and topcoats with respect to their ability to provide good enamel holdout. Primer/topcoat systems with the best enamel holdout will result in desirable gloss in the first coat of topcoat application.

Keywords

absorption; enamel holdout; primer; sealer; under-coater;; ICS Number Code 25.220.50 (Enamels)

To find similar documents by ASTM Volume:

06.02 (Paint -- Products and Applications; Protective Coatings; Pipeline Coatings)

To find similar documents by classification:

25.220.50 (Enamels)

This document comes with our free Notification Service, good for the life of the document.

This document is available in either Paper or PDF format.

Document Number

ASTM-D7786-13(2019)

Revision Level

2013 R19 EDITION

Status

Current

Modification Type

Reapproval

Publication Date

April 1, 2019

Document Type

Test Method

Page Count

3 pages

Committee Number

D01.42