SS-EN-10302 › Creep resisting steels, nickel and cobalt alloys
Document Center Inc. is an authorized dealer of SIS standards.
The following bibliographic material is provided to assist you with your purchasing decision:
The following bibliographic material is provided to assist you with your purchasing decision:
1.1 This European Standard covers the grades of wrought steels and alloys listed in Table 1 and Table 2, which are usually employed for components and equipment, for which the main requirement is their creep resistance under mechanical long-time stressing at temperatures above 500 C. NOTE Heat resisting grades given in EN 10095 [9] may also be used for similar applications if so agreed. 1.2 This European Standard specifies the technical delivery conditions for semi-finished products, for hot or cold rolled sheet/plate and strip, hot or cold formed (cold drawn) bars, rods, wire and sections. 1.3 The general technical delivery conditions specified in EN 10021 apply in addition to the specifications of this European Standard, unless otherwise specified in this European Standard. 1.4 This European Standard does not apply to components manufactured by further processing the product forms listed in 1.2 with quality characteristics altered as a result of such further processing. 1.5 This European Standard shall not be used for aerospace and pressure purposes. 1.6 For steels and alloys with similar chemical composition, but intended for different applications, see the Bibliography.
To find similar documents by classification:
77.120.01 (Non-ferrous metals in general)
77.140.01 (Iron and steel products in general)
77.150.01 (Products of non-ferrous metals in general)
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Designation Name
SS-EN 10302:2008
Revision Level
2008 EDITION
Status
Current
Publication Date
March 31, 2008
Language(s)
English
Page Count
56
International Equivalent
EN 10302:2008(IDT)