ISO-2566-2 › Steel - Conversion of elongation values - Part 2: Austenitic steels
The following bibliographic material is provided to assist you with your purchasing decision:
This document specifies a method of converting room temperature percentage elongations after fracture obtained on various proportional and non-proportional gauge lengths to other gauge lengths.
Formula (1), on which conversions are based, is considered to be reliable when applied to austenitic stainless steels within the tensile strength range 450 to 750 N/mm2 and in the solution treated condition.
These conversions are not applicable to:
a) cold reduced steels;
b) quenched and tempered steels;
c) non-austenitic steels.
These conversions are not applicable when the gauge length exceeds or where the width to thickness ratio of the test piece exceeds 20.
To find similar documents by classification:
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ISO 2566-2:2021
Revision Level
2ND EDITION
Status
Current
Publication Date
Dec. 1, 2021
Committee Number
ISO/TC 17/SC 20