ISO-1126 › Rubber compounding ingredients - Carbon black - Determination of loss on heating
The following bibliographic material is provided to assist you with your purchasing decision:
ISO 1126:2015 specifies methods for determining the loss on heating of carbon black for use in the rubber industry. This loss on heating is due primarily to loss of moisture, but traces of other volatile materials may also be lost.
These methods are not applicable to treated carbon blacks which contain added volatile materials.
One of the following three methods is used:
- method 1: gravity-convection oven method;
- method 2: moisture balance method;
- method 3: infrared irradiation method (rapid method).
Method 1 is the preferred method.
To find similar documents by classification:
83.040.20 (Rubber compounding ingredients Including carbon black, kaolin clay, etc.)
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ISO 1126:2015
Revision Level
5TH EDITION
Status
Current
Publication Date
Sept. 15, 2015
Committee Number
ISO/TC 45/SC 3