Scope
1.1 This practice describes the techniques used for detecting two different polymer entities such as:
1.1.1 Abnormal specks or spots on a surface or in the film that are objectionable as defects and
1.1.2 Layers of different polymeric sheets commonly used as barrier films made by coextrusion.
1.2 This practice utilizes through-transmittance optical and infrared techniques.
1.3 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. Specific hazard statements are given in Section 7.
Note 1: There is no known ISO equivalent to this standard.
1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
Significance and Use
4.1 A speck will ultimately cause a failure to occur by virtue of its appearance in a film or by the decrease in electrical or mechanical properties in the polymer substrate (see Specification D1248).
4.2 The analysis of composite layers for barrier purposes by microscopic Fourier transform infrared spectroscopy (FT-IR) can indicate the adequacy of the barrier tape or indicate why a barrier may be defective (a missing layer or hole in the layer or poor coextrusion practice). Fig. 1 represents a typical multilayer film.
FIG. 1 Position and Function of Materials in a Typical Multilayer Film
Keywords
Fourier transform infrared spectroscopy; microscopy; microsampling; cross-polarized;; ICS Number Code 83.140.20 (Laminated sheets)
To find similar documents by ASTM Volume:
To find similar documents by classification:
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ASTM-D5477-18
Revision Level
2018 EDITION
Status
Current
Modification Type
Revision
Publication Date
Aug. 1, 2018
Document Type
Practice
Page Count
4 pages
Committee Number
D20.70