Scope
1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot.
1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included.
1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded.
1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot.
1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Keywords
breaking strength; fibers; textile fibers; ICS Number Code 59.060.20 (Man-made fibres)
To find similar documents by ASTM Volume:
07.01 (Textiles (I): D76 - D4391)
To find similar documents by classification:
This document comes with our free Notification Service, good for the life of the document.
This document is available in either Paper or PDF format.
Document Number
ASTM-D3217_D3217M-20
Revision Level
2020 EDITION
Status
Current
Modification Type
Revision
Publication Date
July 27, 2020
Document Type
Test Method
Page Count
5 pages
Committee Number
D13.58